Sugar cane hammers with better service life

Informations générales
Nom du centre
SSAB
Description du cas

Description: Second Step crushing in a sugar mill

Technical data: Wear from the frictional heat on the head of the cap. A squeezing / crushing action needed for the fragmentation

Service Life and Status: Hard faced mild steel hammer held one week. New design with shaft in Hardox® 400 and cap in Hardox® 600 holds two weeks.

Further Service life increases will be achieved by a HF(Hard facing) layer on top of the Hardox® 600 cap.  A butter layer of austenitic 307 is needed.

Client final
Domaine d'activités
Industries agricole, forestière et pêche
Matière première traitée
Grains
Pièce d'usure
Équipement
Hammers
Température
0 – 250 °C / 32 – 480 °F
Taille du matériau traité
10 – 300 mm / 0,4 – 12"
Solution
Nouvelle solution
Hardox 600
Facteurs de succès clés
Durée de vie prolongée
100%